Effect of sodium carbonate on alkaline self-leaching of gold …
As the multi-element analysis shown in Table 1, gold-bearing flotation concentrate selected for the study of OPASL are rich with sulphur, iron, silicon and arsenic, which the content is 20.57%, 15.46%, 13.26% and 2.14%, respectively.The content of Au measuring 53.13 g/Mg is relatively high. The main phases of flotation concentrate …